TP304H炉管失效原理及裂解炉对流段蒸汽过热炉管材料选择

刘克刚   

  1. 中国石化工程建设有限公司,北京 100101
  • 收稿日期:2023-03-07 修回日期:2023-04-11 出版日期:2023-06-25 发布日期:2023-07-11
  • 作者简介:刘克刚,男,2009年毕业于大连理工大学化工过程机械专业,工学硕士,长期从事裂解炉设备设计工作,高级工程师。

Failure Mechanism of TP304H Austenitic Stainless Steel Pipe and Material Selection Principle of High Pressure Steam Pipe for Cracking Furnace

Liu Kegang   

  1. SINOPEC Engineering Incorporation, Beijing, P.C. 100101
  • Received:2023-03-07 Revised:2023-04-11 Online:2023-06-25 Published:2023-07-11

摘要: 介绍TP304H炉管的高温失效原理,并将其与多种耐热钢进行性能对比。结合裂解炉对流盘管中蒸汽过热炉管的使用工况特点,提出材料选择的方法和原则,并得出P91304H两种材质耐热钢作为裂解炉蒸汽过热炉管材料的具体使用工况。

关键词: 裂解炉  , 对流盘管  , 失效  , 材料选择

Abstract:

This paper introduces the failure mechanism of TP304H pipe, and compares its high temperature performance with those of several typical heat-resistant steel. Combined with the working condition characteristics of high temperature steam pipes in convection coil of cracking furnace, the material selection method and principle are proposed. The specific working conditions of P91 replacing 304H are provided.

Key words: cracking furnace, convection coil, failure, material selection